PLA is the easiest filament to print and suits most models and prototypes, but softens in heat. PETG is tougher and more heat and moisture resistant, good for functional parts. ABS and ASA handle higher heat and outdoor use, but warp without an enclosure and give off fumes. TPU is flexible for grips and cases. Keep filament dry, since moisture causes stringing and weak parts.
Material choice decides strength, heat resistance and how hard the print is.
Compared
| Filament | Ease | Heat resistance | Strength | Notes |
|---|---|---|---|---|
| PLA | Easiest | Low | Stiff | Most popular |
| PETG | Easy | Medium | Tough | Strings if wet |
| ABS | Harder | High | Tough | Enclosure, ventilation |
| ASA | Harder | High, UV stable | Tough | Outdoor parts |
| TPU | Moderate | Medium | Flexible | Slow printing |
Tips
- Store spools with desiccant or in a dry box.
- Use a hardened nozzle for carbon fiber or glow filaments.
- Check the maker’s temperature range for each spool.
Ventilation
Ventilate when printing ABS and ASA, and consider an enclosure with filtration.
Pick the printer first: FDM vs resin.
Common questions
What filament should I start with?
PLA. It prints at lower temperatures, rarely warps and comes in many colors.
Why does my filament string?
Wet filament is a common cause. Dry it in a filament dryer and store it with desiccant.